Subhajjit solar_cell Pattern BiVO4 Self-assembledMonolayer PetruPoni SrO ThermalDetectors Regensburg C36H74 SICM Co/Cr/Pt AmplitudeModulation Display LateralPFM DataStorage PS_PVAC Lateral Hafnia Photovoltaics piezoelectric force microscopy ScanningIon-ConductanceMicroscopy atomic_steps suspended_graphene Polyethylene Chromium HDD SingleCrystal ScanningKelvinProbeMicroscopy pulsed_laser_deposition Carbon Beads LateralForce Polyimide StyreneBeads
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Polyurethane
Scanning Conditions
- System: NX20
- Scan Mode: Non-contact, TCS
- Cantilever: AC160TS (k=26N/m, f=300kHz)
- Scan Size: 10μm×10μm
- Scan Rate: 0.5Hz
- Pixel: 512×256