Ceramics Grain AlkaneFilm I-VSpectroscopy Bismuth hard_disk_media CHRYSALIS_INC Gong AnodizedAluminumOxide Aggregated_molecules Aluminium_Oxide light_emitting LateralForce Edwin Piranha Inorganic Defect GranadaUniv PolymerPatterns NUS Ito ScratchMode PrCurve Ni81Fe19 HOPG Biology BismuthFerrite MechanicalProperties ElectrostaticForceMicroscopy BlockCopolymer CeramicCapacitor MagneticForceMicroscopy INSPParis Cobalt Croatia
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Magnetic Vortex Core (Ni-Fe alloy)
Scanning Conditions
- System: NX10
- Scan Mode: MFM
- Cantilever: LM-MFMR (k=2.8N/m, f=75kHz)
- Scan Size: 40μm×40μm
- Scan Rate: 0.2Hz
- Pixel: 1024×1024
- Lift Height: 80nm
- Scan Mode: MFM
- Cantilever: LM-MFMR (k=2.8N/m, f=75kHz)
- Scan Size: 40μm×40μm
- Scan Rate: 0.2Hz
- Pixel: 1024×1024
- Lift Height: 80nm