Laser LithiumNiobate Silver Barium_titanate Biofilm LifeScience TempControl biocompatible atomic_layer PvdfFilm Pvdf Sio2 dichalcogenide FloppyDisk INSPParis Change KAIST Perovskite Optical Polyurethane StainlessSteel IVSpectroscopy CompactDisk Bio GlassTemp Foil Liquid Ram dielectric trench Yttria_stabilized_Zirconia BaTiO3 Dental thermal_conductivity HexacontaneFilm TappingMode
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Copper Foil
Scanning Conditions
- System: NX10
- Scan Mode: Non-contact
- Cantilever: AC160TS (k=26N/m, f=300kHz)
- Scan Size: 1μm×1μm
- Scan Rate: 0.5Hz
- Pixel: 512512