IndiumTinOxide lift_mode Vanadate PUR Permalloy Monisha food Barium_titanate Polyaniline Subhajjit Gold Polytetrafluoroethylene Wonseok Chungnam_National_University Croatia SThM HexagonalBoronNitride Lattice Molybdenum PhaseChange temperature_control Tungsten PhaseImaging fluoroaalkane LithiumNiobate HBN Moire Collagen Composite Workfunction C_AFM Kevlar IMT_Bucharest PolyvinylAcetate OrganicCompound
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
HfO2 into Indium Tin Oxide Film
ITO film on 1% HfO2-doped Yttria-stabilized Zirconia (001) orientation grown by pulsed laser deposition. Surface segregation of HfO2 into ITO film.
Scanning Conditions
- System: NX10
- Scan Mode: Non-contact
- Cantilever: AC160TS (k=26N/m, f=300kHz))
- Scan Size: 10μm×10μm,5μm×5μm
- Scan Rate: 0.6Hz, 1Hz
- Pixel Size: 256 × 256, 256 x 256
- Scan Mode: Non-contact
- Cantilever: AC160TS (k=26N/m, f=300kHz))
- Scan Size: 10μm×10μm,5μm×5μm
- Scan Rate: 0.6Hz, 1Hz
- Pixel Size: 256 × 256, 256 x 256