SiliconOxide Wildtype AAO Composition MagneticPhase temperature_control hydrocarbon Mfm Heating thermoplastic_elastomers NusEce StainlessSteel Singapore UTEM Thermal SiWafer Metal-organicComplex #EC PolycrystallineFerroelectricBCZT Varistor TransitionMetal Nanotechnology nanobar F14H20 LithiumNiobate Composite Sadowski TemperatureControlledAFM Bmp BTO MonoLayer MfmAmplitude CarbonNanotube Flake FailureAnalysis
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Kevlar fiber
Scanning Conditions
- System: XE7
- Scan Mode: NCM, F/D mapping
- Cantilever: Diamond probe(k=151N/m, f=50kHz)
- Scan Size:15μm×15μm
- Scan Rate: 0.5Hz
- Pixel: 512×256
- Scan Mode: NCM, F/D mapping
- Cantilever: Diamond probe(k=151N/m, f=50kHz)
- Scan Size:15μm×15μm
- Scan Rate: 0.5Hz
- Pixel: 512×256