F₁₄H₂₀

F₁₄H₂₀ self-assembles into ordered nanostructures because its rigid fluorinated and flexible hydrocarbon segments are immiscible. The 1415 cm⁻¹ signal maps the island-shaped molecular domain.
Scanning Conditions
- Scan Mode: PiFM
- Scan Size: 1 µm×1 µm
- Scan Rate: 0.35 Hz
- Pixel Size: 256×256 pixels
- Probe: NCH Pt/Ir