AtomicLayer Genetic 2d_materials Forevision Ferrite Laser Deposition TCS Conduct IndiumTinOxide STM University_of_Regensburg Typhimurium Polyvinylidene Epoxy DataStorage MolecularSelfAssembly PatternedSapphireSubstrat CuSubstrate TemperatureControlledAFM Chungnam_National_University MechanicalProperties CalciumHydroxide PtfeMembrane ForceVolume Titanate optoelectronics StyreneBeads PS_PVAC AtomicSteps Vinylpyridine Aluminium_Oxide UnivMaryland Graphene OpticalElement
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Polymers
Scanning Conditions
- System: NX10
- Scan Mode: Non-contact
- Cantilever: AC160TS (k=26N/m, f=300kHz)
- Scan Size: 2μm×2μm
- Scan Rate: 1Hz
- Pixel: 512×512
- Scan Mode: Non-contact
- Cantilever: AC160TS (k=26N/m, f=300kHz)
- Scan Size: 2μm×2μm
- Scan Rate: 1Hz
- Pixel: 512×512