StainlessSteel organic_polymer ChemicalCompound DLaTGS PetruPoni C36H74 Piranha PinPointMode Pyroelectric cannabidiol MESA structure Metal-organicComplex ForceVolumeImage SKKU GaN Polydimethylsiloxane HexacontaneFilm WPlug HighResolution BTO Ecoli Hysteresys Bismuth Materials Hydroxyapatite vertical_PFM PyroelectricDetector 2d_materials Tungsten pulsed_laser_deposition self-assembly LogAmplifier DiffractiveOpticalElements #Materials molecule
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Phthalocyanine praseodymium
Scanning Conditions
- System: NX-Hivac
- Scan Mode: SSRM
- Cantilever: CDT-NCHR (k=80 N/m)
- Scan Size: 50μm×50μm, 5μm×5μm
- Scan Rate: 1Hz, 1Hz
- Pixel: 4096×2048, 512×512
- Scan Mode: SSRM
- Cantilever: CDT-NCHR (k=80 N/m)
- Scan Size: 50μm×50μm, 5μm×5μm
- Scan Rate: 1Hz, 1Hz
- Pixel: 4096×2048, 512×512