Silicon TemperatureControllerStage Vanadate Stiffness Typhimurium Polytetrafluoroethylene HDD Hydroxyapatite PUR SurfaceChange Hafnium_dioxide OrganicSemiconductor Patterns Magnetostrictive Wonseok Logo Thermoplastic_polyurethane Piezoelectric graphene_hybrid MolybdenumDisulfide Composite AEAPDES LeakageCurrent Hexatriacontane WS2 Graphene KPFM semifluorinated alkane Optoelectronic Aluminium_Oxide NUS_NNI_Nanocore Glass SKKU MeltingPoint Cobalt
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Stitched image of chiplet
Scanning Conditions
- System : NX-Wafer
- Scan Mode: Non-contact
- Scan Rate : 0.5 Hz
- Scan Size : 100μm×100μm for single image (200μm×200μm stitched image)
- Pixel Size : 512×128 for single image
- Cantilever : OMCL-AC240TS (k=2N/m, f=70kHz)