hydrocarbon neodymium_magnets TyphimuriumBiofilm Hafnium_dioxide PinPointMode MagneticPhase Chungnam_National_University Multiferroic_materials DOE DNAProtein Permalloy IISCBangalore MultiferroicMaterials Ferrite self-assembled_monolayer Phthalocyanine OpticalWaveguides TemperatureControllerStage Optical light_emission Hair ScanningSpreadingResistanceMicroscopy semifluorinated alkane LiIonBattery Metal-organicComplex Array Litho Silver rubber PolyStylene AM_KPFM Materials amplitude_modulation Polydimethylsiloxane Bio
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Li electroplating (deposition) on Cu foil
Scanning Conditions
- System : NX10 in dry room
- Scan Mode: Contact/EC AFM
- Scan Rate : 0.13 Hz
- Scan Size : 30μm×30μm
- Pixel Size : 256×256
- Cantilever : Multi75-G
- ECr : Cu Foil (Working electrode), Li metal (Reference electrode), Li (Counter electrode), 1M LiTFSI in TEGDME (Electrolyte)
- Open circuit voltage : 3.34 VLi/Li+