Battery Domain Water Composition Chemical Vapor Deposition LogAmplifier Bmp Global_Comm Aluminum membrane Lateral_Force_Microscopy UTEM Optical Phthalocyanine LateralForce PhaseImaging Styrene EFMAmplitude MagneticForce ULCA AAO fluorocarbon heterojunctions PvdfFilm temp CompactDisk Fujian Mechinical single_layer Laser Temperature ScanningSpreadingResistanceMicroscopy FailureAnalysis Graphite LiIonBattery
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
2L-MoS₂ (3/3)
Scanning Conditions
- System : FX40
- Sample bias: 0.8 V
- Scan Mode: C-AFM
- Scan Rate : 4 Hz
- Scan Size : 2.5μm×2.5μm
- Pixel Size : 512×512
- Cantilever : ElectricMulti75-G (k=3N/m, f=75kHz)