mechanical property WS2 Tapping FM_KPFM StrontiumTitanate Anneal Gold Varistor CarbonNanotube Galfenol NCM\ PECurve Cobalt-dopedIronOxide China TemperatureControlledAFM SKPM TransitionMetal TappingMode self_healing PUR Memory small_scan Electrode PolycrystallineFerroelectricBCZT UnivCollegeLondon Wildtype 2dMaterials UnivMaryland Polymer molecules Bio PFM Pzt AlkaneFilm vertical_PFM
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Fractals of silver nanoparticles
Scanning Conditions
- System : NX10
- Scan Mode: Non-contact
- Scan Rate : 0.31 Hz, 0.27 Hz
- Scan Size : 50μm2, 40μm2
- Pixel Size : All 256×256
- Cantilever : OMCL-AC160TS (k=26N/m, f=300kHz)