MeltingPoint HydroGel C36H74 Gong LMF Conductive AFM Yttria_stabilized_Zirconia SolarCell SiWafer self-assembled_monolayer multi_layer OxideLayer hydrocarbon FAPbI3 Cell mono_layer Floppy Potential STM Optoelectonics NTU EvatecAG epitaxy Korea Jason membrane China 2dMaterials Chungnam_National_University WPlug SRAM Deposition Wildtype hard_disk piezoelectric force microscopy
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Photoresist pattern (post-development process)
Scanning Conditions
- System : NX-3DM
- Scan Mode: Non-contact
- Scan Rate : 0.1 Hz
- Scan Size : 2μm×10μm
- Pixel Size : 512×2048
- Cantilever : EBD-R2-NCLR (k=45N/m, f=190kHz)