LowDensityPolyethylene Battery MultiLayerCeramicCapacitor INSP LateralForce Styrene Boron non_contact FrictionalForceMicroscopy Annealed MagneticPhase Austenite Pores INSPParis IIT-chennai light_emission Ceramic ElectrostaticForceMicroscopy Biology CHRYSALIS_INC NUS_NNI_Nanocore Potential Ecoli molecules ThermalDetectors PECurve Etch amplitude_modulation fluorocarbon C_AFM Chemical Vapor Deposition Chungnam_National_University LiIonBattery Annealing Conductive AFM
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Bacteria Klebsiella pneumoniae (KP)
Scanning Conditions
- System : NX10
- Scan Mode: Non-contact
- Scan Rate : 0.5 Hz
- Scan Size : 20μm×20μm
- Pixel Size : 256×256
- Cantilever : ContSCR (k=0.2N/m, f=25kHz)