Ferroelectric Magnetic CNT temp Techcomp nanomechanical Moire PolyStylene Hydroxyapatite Mapping Piezoelectric Potential dielectric_trench FAFailureAnlaysis Ecoli Display ScratchMode TungstenDeposition PhaseImaging Fendb Sidewall HexagonalBN cooling Patterns pulsed_laser_deposition Polytetrafluoroethylene sputter TemperatureControllerAFM Heating InorganicCompound BTO OpticalWaveguide ThermalDetectors AdhesionForce GalliumPhosphide
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
PS/LDPE
Spincast layer of PS/LDPE blend on Si.
Scanning Conditions
- System: NX20
- Scan Mode: Tapping
- Cantilever: AD40AS (k=40N/m, f=180kHz)
- Scan Size: 10μm×10μm
- Scan Rate: 0.5Hz
- Pixel Size: 512 × 256
- Scan Mode: Tapping
- Cantilever: AD40AS (k=40N/m, f=180kHz)
- Scan Size: 10μm×10μm
- Scan Rate: 0.5Hz
- Pixel Size: 512 × 256