ElectroChemical TriGlycineSulphate Mechanical&nanotechnology C36H74 Ni81Fe19 NTU 3-hexylthiophene LiftMode RedBloodCell Chemical_Vapor_Deposition CBD CarbonNanotube KevlarFiber Bismuth Aluminum CrAu AmplitudeModulation SSRM MechanicalProperties FuelCell self_healing HiVacuum BTO thermal_property Writing INSPParis GaP LiquidCell Ca10(PO4)6(OH)2 Transparent HighAspect 2d_materials Conductivity dielectric trench Polyvinylidene_fluoride
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Christmas Ball Lithography on Si
Create oxidation layers on bare Si surface using bias mode of lithography.
Scanning Conditions
- System: NX10
- Scan Mode: Lithography
- Cantilever: AD-40-SS (k=40N/m, f=200kHz)
- Scan Size: 40μm×40μm
- Scan Rate: 0.5Hz
- Pixel Size: 1024 × 1024
- Tip Bias: -10V for patterened area
- Scan Mode: Lithography
- Cantilever: AD-40-SS (k=40N/m, f=200kHz)
- Scan Size: 40μm×40μm
- Scan Rate: 0.5Hz
- Pixel Size: 1024 × 1024
- Tip Bias: -10V for patterened area