VerticalPFM plastics DeflectionOptics Dopped Vac Yttria_stabilized_Zirconia Nanofiber Photovoltaics LateralForce DentalProsthesis UnivOfMaryland Jason Cobalt Copolymer Adhesive India Collagen hard_disk TungstenThinFilmDeposition Mfm Blend Oxidation Sapphire contact MechanicalProperties IISCBangalore polymeric_arrays Flake Mechanical Thermal Logo ferromagnetic Cell BreastCancerCell Fe_film
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Composite Barium Titanate
PFM Quad color is overlaid on 3D surface morphology.
Scanning Conditions
- System: NX10
- Scan Mode: PFM
- Cantilever: PPP-ContScPt (k=0.2N/m, f=25kHz)
- Scan Size: 5μm×5μm
- Scan Rate: 0.3Hz
- Pixel Size: 256 × 256