PatternedSapphireSubstrat self-assembly Lattice Pattern Varistor MfmAmplitude epitaxy Yttria_stabilized_Zirconia oxide_layer MagneticForce semifluorinated alkane Piezoresponse Pzt PiezoelectricForceMicroscopy PinPointMode Adhesion atomic_layer Calcium CuParticle TemperatureControl Litho Hafnium_dioxide Carbon Resistance Defects CNT Dopped Thermoplastic_polyurethane CVD Memory CuFoil Photovoltaics Magnetostrictive SelfAssembly Blood
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Suspended single-layer Graphene
Single-layer Graphene is suspended on microchannels fabricated on Si/SiO2 substrate.
Scanning Conditions
- System: NX20
- Scan Mode: Non-contact
- Cantilever: Access-NC (k=113N/m, f=330kHz)
- Scan Size: 40μm×40μm
- Scan Rate: 0.4Hz
- Pixel Size: 256 × 256
- Scan Mode: Non-contact
- Cantilever: Access-NC (k=113N/m, f=330kHz)
- Scan Size: 40μm×40μm
- Scan Rate: 0.4Hz
- Pixel Size: 256 × 256