AtomicSteps F14H20 PS_PVAC Melt Temperature Protein Organic Optoelectonics China Change Hole AM_SKPM Workfunction ForceVolume Steps Worcester_Polytechnic_Institute TemperatureControllerStage DIWafer AnodizedAluminumOxide Polyvinylidene Alloy Perovskite Hafnium_dioxide HexagonalBN Metal-organicComplex Chemical_Vapor_Deposition Korea fluoroaalkane Tape atomic_steps CNT PyroelectricDetector Polyaniline strontiu_titanate Pore
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Collagen film phase change by temp
Scanning Conditions
- System: NX10
- Scan Mode: Tapping
- Cantilever: AC160TS
- Scan Size: 20μm×20μm, 1μm×0.5μm
- Scan Rate: 0.3Hz for 20µm×20µm scan, 1Hz for 1µm×0.5µm scan
- Pixel: 512 × 256 for 20µm×20µm scan, 256 × 128 for 1µm×0.5µm scan
- Scan Mode: Tapping
- Cantilever: AC160TS
- Scan Size: 20μm×20μm, 1μm×0.5μm
- Scan Rate: 0.3Hz for 20µm×20µm scan, 1Hz for 1µm×0.5µm scan
- Pixel: 512 × 256 for 20µm×20µm scan, 256 × 128 for 1µm×0.5µm scan