From elasticity to capillarity in soft materials indentation

Speaker : Michael Kappl Affiliation : Max Planck Institute for Polymer Research, Germany Region : Europe Year : 2018 Language : English Explore the transition from classic plasticity to capillarity in soft materials indentation using laser confocal microscopy. Understand mechanical behavior at nanoscale, offering insights into surface engineering and life science applications.