Position-Specific Attachment of Nanoscale Samples
Speaker : Kai Trepka Affiliation : Harvard University Region : US Year : 2018 Language : English The lecture discusses position-specific attachment methods for nano-scale samples, focusing on optimizing spatial resolution in magnetic force microscopy (MFM). It explores challenges in imaging small biological samples and proposes a strategy involving magnetic nanoparticles and functionalization techniques. Experimental results and potential applications are discussed, along with future research directions.