The Complex Polymers Beneath Your Feet

Speaker : Dr. Nancy A. Burnham Affiliation : Worcester Polytechnic Institute Region : US Year : 2018 Language : English Examine materials science's applications in oil extraction and road infrastructure. Investigate shale's complex polymers for enhanced oil recovery using AFM technology. Analyze evolving microstructures in bitumen for insights into road durability. A scientific exploration at the nexus of technology and materials.