SrO on SrTiO₃ Substrate
An SrO film on an SrTiO₃ substrate was characterized in True Non-contact mode. The image reveals a patterned surface structure with a peak-to-valley height difference of 100.2 nm.
Scanning Conditions
- System: NX20 300mm
- Scan Mode: True Non-contact
- Scan Rate: 0.25 Hz
- Scan Size: 50 µm × 50 µm
- Pixel Size: 512 × 512 pixels
- Peak to Valley: 100.2 nm