Langmuir Blodgett Films and AFM - Wednesday, November 20, 2019
Langmuir–Blodgett (LB) films are nanostructured systems formed when Langmuir films - or monolayers - are transferred from the liquid-gas interface to solid supports during the vertical passage of the support through the monolayers.