Studies of natural rubber (NR) based materials using atomic force microscopy (AFM) technique

Speaker : Dr. Kim Song Tan Affiliation : Malaysian Rubber Board Region : India Year : 2020 Language : English Explore the application of Atomic Force Microscopy (AFM) in studying natural rubber-based materials, focusing on topography, physical properties, and electrical conductivity, crucial for enhancing industrial processes and product development.