Nanoscale Thermal Mapping of Electronic Devices
Speaker : Prof. Miguel Muñoz-Rojo Affiliation : University of Twente, Netherlands Region : China Year : 2020 Language : English The lecture discusses nanoscale thermal mapping of electronic devices using AFM-based techniques. It addresses challenges in electronic devices due to heat dissipation, emphasizing the importance of understanding and managing heat for efficient electronics. The talk explores various thermal measurement techniques, including scanning thermal microscopy (STM), and demonstrates applications in characterizing materials like phase-change memory devices, 2D materials, and conductive bridge memory devices.