Case Snapshot

The Challenge

A quantum materials research team needed a stable near-field optical platform to investigate nanoscale phenomena beyond the diffraction limit.

The Breakthrough

A custom near-field optical microscopy platform built on Park NX10 enabled correlated nanoscale mapping of topography and local optical response.

The Outcome

The team directly visualized propagating surface phonon polaritons and demonstrated tunable dispersion in freestanding SrTiO₃ membranes.

Why It Matters

The work establishes freestanding oxide membranes as a reconfigurable platform for nanoscale photonics and transformation optics.

Unlocking Nanoscale Optical Insights Beyond the Diffraction Limit

University of Minnesota built a custom near-field optical microscopy platform on Park NX10 to visualize and study polaritonic behavior in freestanding 2D oxide membranes.

  • Customer: University of Minnesota, Department of Physics, United States
  • Research Focus: Near-field nanospectroscopy of polaritons in freestanding 2D oxide membranes
  • Solution: Park NX10 as the AFM foundation for a custom near-field optical microscopy platform
  • Key Value: Stable tip–sample control, correlated topographic and optical mapping, and deep-subwavelength visualization of local optical phenomena

The Challenge

Investigating polaritonic behavior in freestanding 2D oxide membranes requires optical measurements far below the diffraction limit while maintaining precise correlation with local topography. The research team needed a stable AFM foundation for a custom near-field optical platform capable of delivering reliable nanoscale measurements.

“Many of the most important optical phenomena in quantum materials occur far below the diffraction limit. To study them reliably, we needed a platform capable of maintaining nanometer-scale stability during near-field optical measurements.”

— Prof. Alex McLeod, School of Physics and Astronomy, University of Minnesota

The Solution

Park NX10 served as the AFM foundation for a custom hyperspectral near-field optical microscopy platform, enabling stable, correlated nanoscale measurements of freestanding 2D oxide membranes.

  • Stable AFM Foundation: Delivered the mechanical stability and precise tip–sample control required for reliable near-field optical measurements.
  • Correlated Nanoscale Mapping: Linked AFM topography with local optical response for accurate interpretation of nanoscale features.
  • Broadband Spectral Mapping: Captured polariton dispersion across the mid-infrared spectral range.
  • Tapping-Mode Near-Field Imaging: Enabled simultaneous AFM topography and near-field optical mapping of polariton behavior beyond the diffraction limit.

The Results

Built on Park NX10, the custom near-field optical platform enabled the team to correlate AFM topography with local optical response at the nanoscale. This made it possible to directly visualize propagating surface phonon polaritons in freestanding SrTiO₃ membranes beyond the diffraction limit.

The measurements also revealed tunable polariton dispersion controlled by membrane thickness and dielectric environment, establishing freestanding oxide membranes as a reconfigurable platform for nanoscale photonics research.

“Near-field nanospectroscopy requires extreme mechanical stability and precise topographic correlation. The Park NX10 platform enabled us to reliably probe optical phenomena far below the diffraction limit with exceptional spatial precision.”

— Prof. Alex McLeod

Key Outcomes

  • Direct visualization of propagating surface phonon polaritons in freestanding SrTiO₃ membranes
  • Correlated nanoscale mapping of AFM topography and local optical response
  • Observation of tunable polariton dispersion through membrane thickness and dielectric environment
  • A promising platform for nanoscale photonics and transformation-optics research

Related Publication

This capability is further demonstrated through peer-reviewed research from the University of Minnesota, including work on interfacial strong coupling and negative dispersion of propagating polaritons in freestanding oxide membranes, published in Advanced Optical Materials. (DOI: 10.1002/adom.202501452)