PinpointPFM ferromagnetic CalciumHydroxide #EC SiliconeOxide ChemicalCompound nanomechanical semifluorinated alkane Holes HighAcpectRatio Tin disulfide CopperFoil Bmp Dental TemperatureControl Ceramic DNAProtein Techcomp SingleCrystal Scratch SelfAssembly Aluminium_Oxide Adhesion HiVacuum KAIST self-assembled_monolayer multi_layer Potential MonoLayer Nanofiber Gallium_Arsenide BismuthVanadate Fujian BoronNitride LaAlO3
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Cast Iron surface change after Corrosion
Scanning Conditions
- System: NX10
- Scan Mode: Contact
- Cantilever: NSC36C (k=0.6N/m, f=65kHz)
- Scan Size: 50μm×50μm
- Scan Rate: 1.5Hz
- Pixel: 512×1024
- EC bias voltage: -0.266V