PyroelectricDetector Temperature self_healing Floppy Adhesive vertical_PFM Flake Varistor Polyvinylidene #EC Molybdenum_disulfide INSPParis ContactModeDots TCS DIWafer plastics ThermalDetectors CalciumHydroxyapatite WS2 temperature_control Polymer StyreneBeads Trench Change Dr.JurekSadowski molecule Magnetic light_emitting MetalCompound thermal_property Copolymer NusEce LiquidImaging Gold Polyurethane
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
HfO2
Scanning Conditions
- System: NX10
- Scan Mode: AM-KPFM
- Cantilever: ElectriMulti75 (k=3 N/m, f=75kHz)
- Scan Size: 10μm×10μm
- Scan Rate: 0.5Hz
- Pixel: 256×256