Cu pad

Scanning Conditions
- System: Park FX200
- Scan Mode: True Non-Contact™ Mode
- Scan Rate: 0.2 Hz
- Scan Size: 50 µm×50 µm
- Pixel Size: 512×512
- Cantilever: SCOUT 350 (k=42 N/m, f=350 kHz)