multi_layer Pore STO Display DomainSwitching cannabis NUS Annealing AIN Thermoplastic_polyurethane Bacteria Inorganic_Compound Chemical Vapor Deposition Heating OxideLayer Polyethylene OrganicSemiconductor Calcium Roughness AtomicLayer Fe_film Ceramic Au111 MoS2 Polymer norganic Metal-organicComplex Terrace biocompatible HOPG FloppyDisk SrTiO3 Biofilm BlockCopolymer Vacuum
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Perovskite
Scanning Conditions
- System: NX10
- Scan Mode: KPFM
- Cantilever: NSC36A Cr-Au (k=1N/m, f=90kHz)
- Scan Size: 4μm×4μm
- Scan Rate: 0.3Hz
- Pixel: 512×256