Chungnam_National_University temp_control InLiquid PolyvinylAcetate PatternedSapphireSubstrat Croatia Wonseok DOE Neodymium Sic FrictionForce LMF flakes block_copolymer CalciumHydroxide Lateral Lanthanum_aluminate heterojunctions NCM\ atomic_steps C36H74 GalliumPhosphide Sadowski Ceramics Celebration Phenanthrene Cross-section align TemperatureControl #Materials CalciumHydroxyapatite Melt INSP Morphology Floppy
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Nanopatterened Graphene on Boron Nitride
Scanning Conditions
- System: NX10
- Scan Mode: Non-contact
- Cantilever: AC160TS (k=26N/m, f=300kHz)
- Scan Size: 4.5μm×4.5μm
- Scan Rate: 0.75Hz
- Pixel Size: 512×512
- Scan Mode: Non-contact
- Cantilever: AC160TS (k=26N/m, f=300kHz)
- Scan Size: 4.5μm×4.5μm
- Scan Rate: 0.75Hz
- Pixel Size: 512×512