PolyStylene optoelectronics SAM ConductingPolymer FastScan silicon_oxide GaN GranadaUniv Co/Cr/Pt Temasek_Lab semifluorinated_alkanes Adhesive temp_control Hole MoirePattern Polypropylene organic_polymer LeakageCurrent Piranha Crystal Composition Zhi Gallium Patterns Barium_titanate Electical&Electronics Phosphide InorganicCompound Pattern CarbonNanotube Al2O3 Strontium GalliumPhosphide Friction Pinpoint PFM
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Polyaniline (PANI)
Scanning Conditions
- System: XE7
- Scan Mode: Non-contact
- Cantilever: ACTA (k=40N/m, f=300kHz)
- Scan Size: 2μm×2μm
- Scan Rate: 0.5Hz
- Pixel: 512×512