Resistance PrCurve nanobar Logo Flake Insulator semifluorinated_alkane DNAProtein LightEmiting MagneticArray Alkane Force-distance Polymer ContactMode P3HT Nanopattern PhaseImaging Permalloy Cell AM_KPFM temp HBN BiVO4 Iron GranadaUniv PVA optoelectronics BoronNitride MfmPhase ScanningTunnelingMicroscopy AAO Hafnia Phase Hexacontane CrAu
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Block copolymer phase change by temp
Scanning Conditions
- System: NX10
- Scan Mode: Tapping,TCS2
- Cantilever: AC160TS (k=26N/m, f=300kHz)
- Scan Size: 5μm×5μm
- Scan Rate: 1Hz
- Pixel: 512×256
- Scan Mode: Tapping,TCS2
- Cantilever: AC160TS (k=26N/m, f=300kHz)
- Scan Size: 5μm×5μm
- Scan Rate: 1Hz
- Pixel: 512×256