Flake PolyvinylideneFluoride Fiber SmallScan Magnetic StyreneBeads temp_control Trench Chemical_Vapor_Deposition Potential H-BN YttriaStabilizedZirconia PANI Dental Pattern SelfAssembly Copolymer blended polymers multi_layer GaN CalciumHydroxide Yeditepe_University Sio2 Chromium Melt SKPM PVAP3HT Al2O3 DNAProtein STM PvdfBead Boron NCM\ Ferroelectric NUS
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Patterned Sapphire Substrate (PSS)
Scanning Conditions
- System: NX10
- Scan Mode: Non-contact
- Cantilever: AR5T-NCHR
- Scan Size: 40μm×40μm, 3μm×3μm
- Scan Rate: 0.3Hz, 1Hz
- Pixel: 256 × 256
- Scan Mode: Non-contact
- Cantilever: AR5T-NCHR
- Scan Size: 40μm×40μm, 3μm×3μm
- Scan Rate: 0.3Hz, 1Hz
- Pixel: 256 × 256