ULCA cannabidiol Display Topography Thermoplastic_polyurethane Wonseok organic_polymer PetruPoni KAIST CeramicCapacitor EFMAmplitude SoftSample C60H122 PinpointNanomechanicalMode IMT_Bucharest Lattice Lateral_Force_Microscopy Varistor Regensburg Chemical_Vapor_Deposition LiftHeight Flake MESA structure FrequencyModulation University_of_Regensburg Conductivity ContactModeDots BismuthFerrite Mechanical Heat PMNPT Hexylthiophene PolyvinylideneFluoride mono_layer Plug
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Magnetic patterned array
Scanning Conditions
- System: NX10
- Scan Mode: MFM
- Cantilever: MFMR (k=2.8N/m, f=75kHz)
- Scan Size: 1.7μm×1.7μm
- Scan Rate:0.5Hz
- Pixel:256×128
- Scan Mode: MFM
- Cantilever: MFMR (k=2.8N/m, f=75kHz)
- Scan Size: 1.7μm×1.7μm
- Scan Rate:0.5Hz
- Pixel:256×128