Alkane Polytetrafluoroethylene aluminum_nitride suspended_graphene Yttria_stabilized_Zirconia FM-KPFM Roughness AAO Ceramics MfmPhase KAIST MfmAmplitude TungstenDeposition Beads Oxidation mechanical_property Composite Water SICM HiVacuum BismuthVanadate AnodizedAluminumOxide Gong food semifluorinated_alkane polymeric_arrays HanyangUniv cannabinoid AlkaneFilm Ca10(PO4)6(OH)2 Electrical&Electronics LateralPFM Fiber Growing MagneticArray
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Gold(111) coated mica substrate
Scanning Conditions
- System: XE7
- Scan Mode: Contact
- Cantilever: PPP-ContScR (k=0.2N/m, f=25kHz)
- Scan Size: 5μm×5μm
- Scan Rate: 1Hz
- Pixel: 256×256
- EC electrode: Ag/AgCl2(Reference electrode), Pt(Counter electrode), CuSO4(0.1mM) + H2SO4(0.01mM)(Electrolyte)
- EC bias voltage: -0.3V