KPFM non_contact IcelandSpar GranadaUniv SPMLabs FailureAnlaysis ChemicalCompound cross section LateralPFM Topography IRDetector ThermalConductivity FrequencyModulation DLaTGS PS_LDPE Genetic AAO Sulfur MechanicalProperty Lift ScanningIon-ConductanceMicroscopy ScanningTunnelingMicroscopy PtfeFilter CalciumHydroxyapatite DIWafer nanomechanical HighAspect NusEce FrictionalForceMicroscopy ElectroDeposition Thermal LightEmiting ShenYang aluminum_nitride SicMosfet
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Li ion battery electrode
Scanning Conditions
- System: NX-Hivac
- Scan Mode: SSRM
- Cantilever: CDT-NCHR (k=80 N/m)
- Scan Size: 50μm×50μm
- Scan Rate: 1Hz
- Pixel: 4096×2048