Conductance Iron Fendb Magnetostrictive PolyvinylAcetate Nanostructure MolybdenumDisulfide IMT_Bucharest Tin disulfide Electrical&Electronics Sperm pinpoint mode single_layer MagneticForce graphene_hybrid Conductive AFM Filter Inorganic_Compound semifluorinated_alkanes Silver FAPbI3 ContactModeDots Blend molecule ferromagnetic Cancer molecules Indent Sulfur molecular_beam ULCA AM_SKPM PtfeFilter InsulatorFilm CBD
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
MoS2
Scanning Conditions
- System: NX10
- Scan Mode: AM-KPFM
- Cantilever: ElectriMulti75 (k=3 N/m, f=75kHz)
- Scan Size: 10μm×10μm
- Scan Rate: 0.5Hz
- Pixel: 256×256