Domain Bacteria Imprint Metal-organicComplex FloppyDisk Calcite Boron Silver Copolymer BaTiO3 PolyStylene Boundary ScratchMode Celebration SrO TemperatureControllerStage PFM CVD CntFilm Tungsten_disulfide DataStorage IRDetector Array Sio2 ContactMode LiIonBattery solar_cell cannabinoid SelfAssembly SoftSample Varistor BreastCancerCell epitaxy BFO self-assembly
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
HOPG Moire
Scanning Conditions
- System: NX10
- Scan Mode: STM
- Cantilever: Pt wire
- Scan Size: 2.5μm×2.5μm, 0.5μm×0.5μm, 0.2μm×0.2μm
- Scan Rate: 0.3Hz, 1Hz, 2Hz
- Pixel: 512×256, 512×256, 256×128
- Scan Mode: STM
- Cantilever: Pt wire
- Scan Size: 2.5μm×2.5μm, 0.5μm×0.5μm, 0.2μm×0.2μm
- Scan Rate: 0.3Hz, 1Hz, 2Hz
- Pixel: 512×256, 512×256, 256×128