Electical&Electronics Global_Comm OrganicCompound Heating Scratch ScanningSpreadingResistanceMicroscopy AlkaneFilm Zagreb Hexylthiophene PolyvinylideneFluoride TempControl membrane RedBloodCell MultiLayerCeramicCapacitor ScanningTunnelingMicroscopy Yttria_stabilized_Zirconia Polymer Patterns Mechanical MBE Epoxy Fet FAPbI3 MolecularSelfAssembly VerticalPFM BiFeO3 Cobalt Vanadate Platinum Optical Phthalocyanine OpticalElement AtomicLayer PinpointPFM MagneticArray
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Phthalocyanine praseodymium
Scanning Conditions
- System: NX10
- Scan Mode: EFM
- Cantilever: PPP-EFM (k=2.8 N/m, f=75kHz)
- Scan Size: 20μm×20μm
- Scan Rate: 0.3Hz
- Pixel: 1024×256