FuelCell Array block_copolymer CastIron I-VSpectroscopy Silver Terrace Zagreb Praseodymium MESA structure Polyvinylidene Piezoelectric Metal-organicComplex Piranha Deposition Hexylthiophene OrganicSemiconductor OpticalElement Sperm TyphimuriumBiofilm neodymium_magnets Dental GaP Optoelectonics CrossSection CuSubstrate ItoGlass Battery Graphite SKKU CuFoil self-assembled_monolayer Thermal chemical_compound ScanningTunnelingMicroscopy
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Si nanowire on glass
Scanning Conditions
- System: XE7
- Scan Mode: SThM
- Cantilever: Thermal probe (k=0.25N/m)
- Scan Size: 3.5μm×3.5μm
- Scan Rate: 1Hz
- Pixel: 512×256
- Scan Mode: SThM
- Cantilever: Thermal probe (k=0.25N/m)
- Scan Size: 3.5μm×3.5μm
- Scan Rate: 1Hz
- Pixel: 512×256