GaP single_layer FrictionalForceMicroscopy CVD PECurve Dr.JurekSadowski Self-assembledMonolayer Vanadate CaMnO3 BariumTitanate ContactModeDot exfoliate KPFM membrane Bacterium blended polymers Vac EPFL LateralPFM Polypropylene conductive Temperature TyphimuriumBiofilm Titanate SoftSample molecules Mechanical&nanotechnology Varistor ScanningIon-ConductanceMicroscopy Vortex AEAPDES Morphology PolymerPatterns Multiferroic_materials MolybdenumDisulfide
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
MoS2
Scanning Conditions
- System: NX10
- Scan Mode: AM-KPFM
- Cantilever: ElectriMulti75 (k=3 N/m, f=75kHz)
- Scan Size: 10μm×10μm
- Scan Rate: 0.5Hz
- Pixel: 256×256