ScanningSpreadingResistanceMicroscopy Step Cobalt-dopedIronOxide SKPM pulsed_laser_deposition OrganicSemiconductor ForceVolume YszSubstrate CP-AFM TungstenDeposition self_healing AM_SKPM Regensburg Leakage TriGlycineSulphate Reduction Floppy dielectric_trench HexacontaneFilm PtfeFilter Hysteresys plastic BaTiO3 BariumTitanate Alkane hard_disk Mechanical Ecoli thermal_conductivity I-VSpectroscopy PyroelectricDetector Boundary Lateral Aluminium_Oxide PS_LDPE
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Block copolymer phase change by temp
Scanning Conditions
- System: NX10
- Scan Mode: Tapping,TCS2
- Cantilever: AC160TS (k=26N/m, f=300kHz)
- Scan Size: 5μm×5μm
- Scan Rate: 1Hz
- Pixel: 512×256