Modulus ring shape fluorocarbon ForceDistanceSpectroscopy OxideLayer NTU 2d_materials Neodymium LogAmplifier StrontiumTitanate flakes TiO2 TempControl FAPbI3 Conductivity electrospinning LFM Korea Annealing I-VSpectroscopy BTO FrictionalForceMicroscopy Laser LiNbO3 Chungnam_National_University Temperature Electronics lift_mode Aggregated_molecules Phenanthrene DentalProsthesis ConductiveAFM Varistor Heating Ceramics
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Block copolymer ; Fast scan
Scanning Conditions
- System: NX10
- Scan Mode: Tapping
- Cantilever: AC55TS (k=85N/m, f=1600kHz)
- Scan Size: 0.5μm×0.5μm
- Scan Rate: 6Hz, 13Hz
- Pixel: 256×256
- Scan Mode: Tapping
- Cantilever: AC55TS (k=85N/m, f=1600kHz)
- Scan Size: 0.5μm×0.5μm
- Scan Rate: 6Hz, 13Hz
- Pixel: 256×256