#Materials CopperFoil Optoelectronic Cancer ForceDistanceSpectroscopy STO Hysteresys ScratchMode amplitude_modulation LiftHeight Formamidinium_lead_iodide Sperm Multiferroic_materials Deposition Ni81Fe19 University_of_Regensburg high_resolution VinylAlcohol Mechanical&nanotechnology Calcite plastic Step align Bmp Tungsten_disulfide Current FM-KPFM MechanicalProperty Chungnam_National_University SKPM Mapping Yttria_stabilized_Zirconia Tin disulfide AIN CeramicCapacitor
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Polymers
Scanning Conditions
- System: NX10
- Scan Mode: Non-contact
- Cantilever: AC160TS (k=26N/m, f=300kHz)
- Scan Size: 2μm×2μm
- Scan Rate: 1Hz
- Pixel: 512×512
- Scan Mode: Non-contact
- Cantilever: AC160TS (k=26N/m, f=300kHz)
- Scan Size: 2μm×2μm
- Scan Rate: 1Hz
- Pixel: 512×512