PatternedSapphireSubstrat biocompatible CopperFoil StrontiuTitanate BismuthVanadate Aluminium_Oxide SICM Pinpoint PFM Magnetic Force Microscopy Varistor Oxidation Pinpoint flakes Bio Gold SrO BiVO4 Temperature SPMLabs Zagreb LateralForceMicroscopy FloppyDisk self_assembly HOPG MoS2 Composition ShenYang domain_switching LMF LightEmiting Ca10(PO4)6(OH)2 optoelectronics Device Conductance Celebration
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Polymer patterns on Si (2/2)
Scanning Conditions
- System: NX10
- Scan Mode: KPFM
- Cantilever: NSC36Cr-Au (k=1N/m, f=90kHz)
- Scan Size: 10μm×10μm
- Scan Rate: 0.2Hz
- Pixel: 512×256