Anneal FFM Cobalt-dopedIronOxide Biofilm KelvinProbeForceMicroscopy Oxide optoelectronics PhaseChange phase_change ScanningTunnelingMicroscopy LiquidCrystal StrontiuTitanate OpticalWaveguides Hafnium_dioxide Workfunction KAIST LogAmplifier graphene_hybrid PhaseImaging fifber Ceramic OxideLayer Hole Bacteria single_layer Domain LifeScience SThM Scanning_Thermal_Microscopy Mobile ito_film CeramicCapacitor Water Thermal mfm_amplitude
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
BiVO4 on treated YSZ substrate
Scanning Conditions
- System: NX10
- Scan Mode: Non-contact
- Cantilever: AC160TS (k=26N/m, f=300kHz)
- Scan Size: 10μm×10μm
- Scan Rate: 0.36Hz
- Pixel: 256×256