Celebration Graphene multi_layer Monisha Fluoride non_contact Austenite ImideMonomer KelvinProbeForceMicroscopy semifluorinated_alkanes DNA Molybdenum_disulfide Annealing NUS_Physics HardDiskMedia Dental Wildtype Vinylpyridine vertical_PFM Thermoplastic_polyurethane SolarCell Glass medical GalliumPhosphide mono_layer silicon_oxide NtuEee CarbonNanotube CompactDisk SThM Worcester_Polytechnic_Institute Mapping doped PDMS Epoxy
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
ExFoliated graphene on SiO₂/Si wafer
Scanning Conditions
- System : FX40
- Scan Mode: Non-Contact, Lithography
- Scan Rate : 1 Hz
- Scan Size : 10μm×10μm
- Pixel Size : 256×256
- Cantilever : PPP-EFM (k=2.8N/m, f=75kHz)
- Litho. Condition : Force 200nN, Writing speed 0.2 μm/s , AC bias 10 V @ 40 kHz, Humidity ~90% RH