Varistor GlassTemp LightEmission AM-KPFM Transparent EFM Conductive AFM Cobalt-dopedIronOxide Cell ShenYang IRDetector phase_change cannabinoid Magnets semifluorinated alkane SAM Fiber Subhajjit Carbon Chemical Vapor Deposition PtfeMembrane Formamidinium_lead_iodide Thermal Christmas cooling Global_Comm Self-assembledMonolayer ScanningKelvinProbeMicroscopy Au111 ferromagnetic oxide_layer Thermoplastic_polyurethane SSRM ChemicalCompound high_resolution
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Monolayer Graphene on PDMS Surface
Monolayer Graphene grown on Cu foil using CVD process is transferred on to PDMS substrate.
Scanning Conditions
- System: NX20
- Scan Mode: Tapping
- Cantilever: Access-NC (k=113N/m, f=330kHz)
- Scan Size: 100μm×100μm
- Scan Rate: 0.6Hz
- Pixel Size: 256 × 256
- Scan Mode: Tapping
- Cantilever: Access-NC (k=113N/m, f=330kHz)
- Scan Size: 100μm×100μm
- Scan Rate: 0.6Hz
- Pixel Size: 256 × 256